필라멘트 와인딩 공법 시 Helical/Hoop 교차 적층 설계에 따른 HNT-CFRP 복합재 파이프의 나노입자 강화효과 및 수환경 특성에 관한 연구

DC Field Value Language
dc.contributor.advisor 김윤해 -
dc.contributor.author 최지수 -
dc.date.accessioned 2021-01-31T08:40:29Z -
dc.date.available 2021-01-31T08:40:29Z -
dc.date.issued 2020 -
dc.identifier.uri http://repository.kmou.ac.kr/handle/2014.oak/12551 -
dc.identifier.uri http://kmou.dcollection.net/common/orgView/200000342084 -
dc.description.abstract Fiber-reinforced composite materials have lower specific strength and specific gravity compared to metal materials. In addition, it has great durability, corrosion resistance so it was widely used in the aircraft, automotive, marine, marine and energy industries. Composite materials are also applied to shell-like structures such as pipes and pressure vessels based on formability and strength. In particular, research is being actively conducted to replace metal pipes with FRP pipes. FRP pipes can be produced through a variety of composite manufacturing processes. In particular, the filament winding process is mainly used for manufacturing pipes with high strength and fracture stability. Since the filament winding process can freely design a winding pattern, it is possible to manufacture a pipe suitable for the use environment. In general, a helical winding pattern is mainly used for excellent strength and to suppress the outflow of liquid or gas. However, the pipe of the helical winding pattern has a risk of completely cutting the entire cylinder after buckling so it is necessary to properly mix and use the helical pattern and the hoop pattern. FRP pipes have an advantage that they do not corrode differently from metallic materials and have great chemical resistance. For this reason, it can be used in special environments such as water and sewage, industrial water, related water, ships, oil transportation, water storage, fire hydrant piping steel pipe, city gas, and liquefied petroleum gas supply steel pipe. In particular, steel pipes require a huge amount of time and cost to install and paint facilities, and to repair facilities due to aging. Therefore, FRP pipes are being developed to replace them. FRP is suitable for use in water but environmental degradation occurs in which the matrix material is separated from the strengthening agent. These factors directly affect strength degradation. Therefore, in this study, in order to increase the durability of the FRP pipe, the nanoparticles having a property of controlling the absorption of moisture were added to the manufacturing process of the pipe. So in this study, a method of adding a hoop pattern and adding HNT to a helical pattern was used to fabricate a CFRP pipe suitable for use in an underwater environment with high strength. CFRP pipe specimens with two parameters were evaluated through bending test, interlaminar shear strength test, compression test, and moisture absorption rate analysis. As a result, the addition of a hoop pattern with a thickness corresponding to 8% of the helical pattern showed the most high mechanical strength through efficient transmission of bending and compression loads. Further hoop patterns have been shown to cause delamination of the helical and hoop layers. When the added HNT was evenly dispersed at the interface of the two patterns, the adhesion of the interface was increased to suppress the occurrence of peeling, which was most effective when the mass of the added HNT was 0.5%. -
dc.description.tableofcontents 1. 서 론 1 1.1 연구의 배경과 필요성 1 1.2 연구의 목적 4 2. 문헌 고찰 7 2.1 CFRP 파이프의 제작 공정 7 2.1.1 필라멘트 와인딩 공정(Filament winding process) 7 2.1.2 필라멘트 와인딩 공정의 분류 8 2.2 나노 복합재료(Nanocomposites) 10 2.2.1 나노 기술 10 2.2.2 할로이사이트 나노튜브가 첨가된 나노고분자복합재료 12 3. 실험재료 및 방법 14 3.1 실험재료 14 3.1.1 탄소 섬유(Carbon fiber) 14 3.1.2 할로이사이트 나노튜브(Halloysite nanotube; HNT) 16 3.1.3 할로이사이트 나노튜브의 분산 18 3.2 필라멘트 와인딩 공정을 이용한 CFRP 파이프 제작 20 3.2.1 CFRP 파이프의 패턴 설계 20 3.3 기계적 특성 시험 24 3.3.1 굽힘 시험(Bending test) 24 3.3.2 층간 전단 강도 시험(Inter laminar shear strength test) 24 3.3.3 압축 시험(Compressive test) 25 3.4 수분 흡수 거동에 따른 환경 특성 시험 26 3.5 적층면 분석 28 4. 실험결과 및 고찰 29 4.1 기계적 물성 시험 결과 29 4.1.1 굽힘 시험 결과 29 4.1.2 층간 전단 강도 시험 결과 39 4.1.3 압축 시험 결과 46 4.2 환경 특성 실험 결과 49 4.2.1 수분 흡수 거동 49 4.2.2 흡습에 의해 발생한 기계적 물성 열화 53 4.3 고찰 62 5. 결론 64 감사의 글 67 참고문헌 68 -
dc.format.extent 73 -
dc.language kor -
dc.publisher 한국해양대학교 대학원 -
dc.rights 한국해양대학교 논문은 저작권에 의해 보호받습니다. -
dc.title 필라멘트 와인딩 공법 시 Helical/Hoop 교차 적층 설계에 따른 HNT-CFRP 복합재 파이프의 나노입자 강화효과 및 수환경 특성에 관한 연구 -
dc.title.alternative Analysis of nanoparticle strengthening effect and water absorption behavior on Helical/Hoop cross-laminated HNT-CFRP composite pipe using filament winding -
dc.type Dissertation -
dc.date.awarded 2020. 8 -
dc.contributor.alternativeName Choi Ji su -
dc.contributor.department 대학원 조선기자재공학과 -
dc.contributor.affiliation 한국해양대학교 대학원 조선기자재공학과 -
dc.description.degree Master -
dc.identifier.bibliographicCitation 최지수. (2020). 필라멘트 와인딩 공법 시 Helical/Hoop 교차 적층 설계에 따른 HNT-CFRP 복합재 파이프의 나노입자 강화효과 및 수환경 특성에 관한 연구 -
dc.subject.keyword 필라멘트 와인딩 공정 -
dc.subject.keyword 와인딩 패턴 -
dc.subject.keyword 탄소섬유 복합재 파이프 -
dc.subject.keyword 할로이사이트나노튜브 -
dc.subject.keyword 나노 복합재료 -
dc.contributor.specialty 재료공학과 -
dc.identifier.holdings 000000001979▲200000001758▲200000342084▲ -
Appears in Collections:
조선기자재공학과 > Thesis
Files in This Item:
필라멘트 와인딩 공법 시 Helical_Hoop 교차 적층 설계에 따른 HNT-CFRP 복합재 파이프의 나노입자 강화효과 및 수환경 특성에 관한 연구.pdf Download

Items in Repository are protected by copyright, with all rights reserved, unless otherwise indicated.

Browse